Влияние состава электролита на образование пероксида водорода и выброс металла при микроразряде на алюминиевом аноде
Сырьева Анна Викторовна, Калинина Татьяна Анатольевна, Сизиков Анатолий Михайлович et al. · Herald of Omsk University Series Psychology · 2009
It were studied characteristics of anode microdischarges in tetraboric and carbonate solution. In case of aluminic anode usage is observed the spitting of metal into solution, the concentration of hydrogen peroxide is also observed. The containing of discharge secondary products depends on the electrolyte composition, particularly it depends on the concentration of Na2C03 or Na2B407 in the solution. The quantity of produced products in the tetraboric solutions is determined by energy parameter of microdischarges, which depends on the electrolyte concentration. In the carbonate solutions is produced less hydrogen peroxide, because the carbonate ion is an OH-radical scavenger. The dissolution of the porous part of oxide layer in the carbonate solutions results the bigger accumulation of aluminic ion in the solution than by the rupture.
Cited by 0 works.