铝合金热轧带材“中凸度超标+中间波浪”板形缺陷的原因分析与改进措施
陈祚启, 广西柳州银海铝业股份有限公司, 高作文 et al. · 铝加工 · 2014
middle of the crown superscalar + wave of the defect resulted from 5182 aluminum alloy produced by single twin winding four-high reversing hot rolling mill was researched experimentally, the results show that the defects are caused because the original work roll crown is too small and pass reduction is unreasonable, emulsion spraying pressure is too small. The defects can be deleted by increasing the original work roll crown, optimization pass reduction, improving emulsion spray pressure .