Исследование релаксации заряда в пленках ударопрочного полистирола с включениями диоксида титана

Гороховатский Юрий Андреевич, Гулякова Анна Александровна · Izvestia Herzen University Journal of Humanities & Sciences · 2011

The charge relaxation processes in pure high-impact polystyrene films (HIPS) and HIPS filled with titanium dioxide (TiO2) inclusions of rutile modification are investigated by means of the combination of dynamic-mechanical and dielectric methods: thermally stimulated depolarization current (TSDC) measurements, dielectric relaxation spectroscopy (DRS), dynamic mechanical analysis (DMA) and differential scanning calorimetry (DSC). The TSDC and the dielectric spectra show two well separated relaxation regions. The lower-temperature process appears in all films and can be attributed to the glass transition in HIPS as proved by DSC and DMA measurements. It is not influenced by addition of TiO2. The higher-temperature process is observed only for composite films, and the magnitudes of the corresponding TSDC or dielectric loss-factor peaks increase with increasing filler content. It is assumed to be related to charge migration at the polymer-filler interface due to the Maxwell-Wagner effect. For this process the values of most probable activation energy and effective frequency factor of EAD were determined using Tikhonov regularization method: W = 1,1 e V, ω = 1011 s-1.

Cited by 0 works.

Authors