환경조건이 알칼리-실리카 반응에 의한 모르타르 봉 길이 팽창에 미치는 영향
김성권, 윤경구, 홍승호 et al. · 한국도로학회논문집 · 2011
The possibility of ASR(alkali-silica reaction) for coarse aggregates had known to be low up to recently in Korea. But the distress of ASR was identified and reported by ASTM C 1260 test. The purpose of this paper was to identify the effect of environmental conditions on length expansion of mortar-bar by alkali-silica reaction with KS F 2546 and ASTM C 1260 test. The results of this study were as following; The result of KS F 2546 test for five kinds of aggregates shows that all of them are non-reactive. But that of ASTM C 1260 test shows that all of aggregates except Andesite-2 are over possible reactive because of environmental condition such as external alkali ion by 1N NaOH, high temperature and humidity. The result of variety of NaOH concentration on ASTM C 1260 using Siltstone indicates that length expansion rate increases highly as NaOH concentration increases. And, comparison results of KS F 2546 for Siltstone with that of 0.00N NaOH experiment indicates that length expansion rate increases as temperature and humidity increases.
Cited by 0 works.