혼화재 종류 및 치환율 변화에 따른 콘크리트의 응결 및 강도발현 특성
김종, 송승헌, 전충근 et al. · 대한건축학회 학술발표대회 논문집 - 구조계 · 2004
In this paper, the results of setting and strength properties of concrete incorporating cement kiln dust, fly ash and blast furnace slag respectively are reported in order to reduce hydration heat of mass concrete and achieve economical advantage. According to test results, setting time was not affected by CKD contents, whereas The use of FA with 10 and 20% retarded the setting time more than 2 hours and 30% more than 3hours. The increase of BS with 20 and 40% delayed setting time more than 1.5 hours and 60% of BS, 4hours. For compressive strength, the increase of CKD reduced the compressive strength. The use of CKD with 10% had little effect on strength gain. The use of FA and BS resulted in a reduction in compressive strength in proportion to the contents at early age. At 28days, compressive strength with FA and BS exhibited a parabola curve with an increase in FA and BS contents. Higher strength gain was achieved in 10% of FA and 20% of BS at 28days. It can be seen that the use of mineral admixture in mass concreting considering placing layer can reduce hydration heat and economical advantage.
Cited by 0 works.