기량검증용 결함시험편 제작 및 초음파특성 평가

홍재근, 박지홍, 손영호 et al. · 대한기계학회 춘추학술대회 · 2003

Performance demonstration with real flawed specimens has been strongly required for nondestructive evaluation of safety class components in nuclear power plant. Mechanical or thermal fatigue crack and inter-granular stress corrosion cracking could be occured in the in-service nuclear power plant and mechanical fatigue crack was selected to study in this paper. Specimen was designed to produce mechanical fatigue flaw under tensile stress. The number of cycle and the level of stress were controlled to obtain the desired flaw roughness. After exact physical measuring of the flaw size and location, fracture surface was seal welded in place to establish designed location and size. The remaining weld groove was then filled by using gas tungsten arc welding(GTAW) and flux cored arc welding(FCAW). The results of radiographic testing and ultrasonic testing showed that fatigue cracks were consistent with designed size and location in the final specimens.

Cited by 1 works.