The consolidation of nanosized pure tungsten carbide and carbide alloy powders by spark plasma sintering has been studied. Pure WC sintering modes within the temperature interval (1400–1950)C and heating rates from 25 to 2400C/min have been investigated. Nanostructured specimens with a record hardness of 3180 HV and a satisfactory fracture toughness of K1c=4.5–6.5 MPam1/2 have been obtained. The article determines the dependences of density, hardness, and grain structure of WC-8 wt.% Co alloys with TaC/VC inhibitors on the sintering temperature, heating rate and solid-state sintering time. Nanostructured WC-8 wt.% Co specimens with high values of hardness (17–19 GPa) and fracture toughness (more than 10 MPam1/2) have been obtained.