열압밀화를 이용한 낙엽송의 표면경도 개선

황성욱, 박상범, 서진석 et al. · 한국가구학회지 · 2012

This study was conducted to investigate the surface hardness of thermally-compressed larch wood by compression set and temperature. The surface hardness of thermally-compressed larch wood increased with increasing compression set and temperature. For compression set 60%, the specific gravity was increased as 0.93. However, the surface hardness was lower value as 31.1 N/㎟ compared with a similar specific gravity of the tropical timber. For density profile, less than compression set 40%, compression was observed mainly surface area. On the other hand, more than 50%, density profile variation was reduced by compression of central part. Results of this study indicate that thermally-compressed larch wood can be replace some imported hardwoods such as oak or cherry. However, thermally-compressed larch wood was difficult to replace the tropical timber being imported in terms of surface hardness.

Cited by 0 works.