고온가속열화에 따른 고분자절연재료의 열화특성에 관한 연구
임경범 · 한국화재소방학회 학술대회 논문집 · 2009
An object of the present study is to induce a degradation mechanism by heat degradation of the epoxy glass fiber which is a polymeric material for outdoor. In order to analyze the degradation process of epoxy/glass fiber for outdoor condition, FRP laminate was exposed to high temperature. Then, the degradation process was evaluated by surface potential, surface resistivity, comparing contact angle and XPS. The result of experiments showed that thecharacteristics of the contact angle, surface resistance rate, and surface potential attenuation were improved up to 200℃ of the heat treatment temperature, but were reduced when the heat treatment temperature was higher than 200℃. These phenomena show the existence of hydrophobic surface. Also, as a result of XPS analysis, the relative peak of carbon was shown to be high as the amount of oxygen was reduced up to 200℃ at which the hydrophobic transformation of the surface was progressed, and it was confirmed that the ether (-CO) radical was the main reason for coloring due to heat treatment.
Cited by 0 works.