원자로 용기 외벽 냉각을 통한 차세대 원전 관통부의 건전성 평가를 위한 지속 가열 실험 연구

강경호, 박래준, 민병태 et al. · 대한기계학회 춘추학술대회 · 2002

Under the same induction heating power histories, two tests named as KNGR-SUS-DRY and KNGR-SUS-EXT were performed varying the cooling conditions at the outer surface of the lower head vessel. The maximum heat flux imposed to the inner surface of the lower head vessel was about 0.35 MW/m2 in both the tests. In the KNGR-SUS-DRY test performed without the external vessel cooling, the inner surface of the lower head vessel was ablated by the thickness of 45 mm, which indicated the total ablation of the welding material. Although the welding material was ablated in all, the penetration tube was not ejected outside the lower head vessel due to the thermal expansion of the lower head vessel and the penetration tube. In the KNGR-SUS-EXT test performed with the external vessel cooling, however, the thickness of the ablation is about 10 mm at most.

Cited by 1 works.

Authors