다양한 환경에서의 오스테나이트계 고망간강 용접부 피로거동

정대호, 권재기, 우남섭 et al. · 대한기계학회 춘추학술대회 · 2014

In the present study, the fatigue crack propagation (FCP) behaviors of Fe24Mn (Fe-24Mn-4Cr) in various environments were examined in the different locations of base metal (BM), weld metal (WM) and fusion line (FL) at 298 and 110K and in artificial seawater under various cathodic protection potentials. The FCP rates of Fe24Mn BM specimen was substantially reduced with decreasing temperature from 298 to 110K over the entire ?K regime. The CP potential of -850 and -1,050 mV SCE suppressed the environmental effect of seawater on the FCP behavior of Fe24Mn BM and WM specimens, showing almost identical da/dN-?K curves for both air and seawater environments. The FCP behaviors of Fe24Mn in various environments were discussed based on the microstructural and the fractographic observations.