금속의 표면처리가 다양한 치과용 비귀금속 - 세라믹 시스템의 결합강도에 미치는 영향

황성식, 이해형, 이중배 et al. · 대한치과재료학회지 · 2011

The purpose of this study was to investigate the bond strength of Be-free Ni-Cr base metal alloys with dental porcelain in comparing with those of Be-containing base metal alloys. Alloys used in this study were as followings; for Be-containing alloy, Verabond (VB), Rexillium V (RV); for Be-free alloy, Verabond 2V (2V), Bellabond Plus (BP), Super 3 (S3), Tilite P (TP), Tilite S (TS). Before applying dental porcelain, alloy specimens subjected to two different surface treatments; sandblasting and degassing after sandblasting. Metal-ceramic bond strength was determined from ISO 9693 three-point bending test. Elastic modulus of metal substrate was determined from load-displacement curve obtained from subsequent loading after debonding test. Two-way ANOVA test was conducted to analyze the effect of metal alloy and surface treatment on the bond strength and their interaction. Then multiple comparisons test between group under each surface treatment and t-test between surface treatments were conducted. The metal-ceramic bond strength was significantly affected by difference in alloy used and surface treatment, and the interaction of both variances was also significant (P treatment. Overall, there was no significant difference in the metal-ceramic bond strength between Be-free and Be-containing alloys and the mean bond strength values were recorded over the minimum requirement of ISO 9693 (25 MPa), In conclusion, to increase the metal-ceramic bond strength, method of surface treatment for Ni-Cr base metal alloy should be properly selected before layering of dental porcelain.

Cited by 0 works.

Authors