Активирование спекания оксидной керамики добавками нанодисперсных порошков
Сергей Вениаминович Матренин, Ильин Александр Петрович, Л. О. Толбанова et al. · Известия Томского политехнического университета. Инжиниринг георесурсов · 2010
Ceramic sintering on the basis of Al2O3 and ZrO2, activated byadditives of nanopowders Al2O3 and Al has been studied. It was shown that additive of nanopowder Al2O3 to 20 wt. % into coarse powder α-Al2O3 activated alumina ceramic sintering: its density and microhardness increased. The possibility of obtaining sintered ceramic from nonstabilized ZrO2 by introducing not less than 10 wt. % Al nanopowder additive into initial nanopowder ZrO2 was ascertained. Sinteringpressings from ZrO2 nanopowders with the additive of 20 wt. % Al nanopowder in ammoniac glow discharge plasma the ceramic material with signified inhomogeneous chemical and phase composition and different microstructure was obtained.
Cited by 0 works.