사이알론 세라믹스의 균열치유에 관한 연구
문석재, 박승원, 안석환 et al. · 한국동력기계공학회 학술대회 논문집 · 2008
Sialon was produced by hot-pressing the mixtures of Si 3 N 4 , AIN and Y 2 O 3 powders. Fracture toughness and Vickers hardness of smooth specimen were average 7.05 MPa·m 0.5 and Hν = 1580, respectively. Density of three kinds of specimens, smooth specimen, smooth and healed specimen, smooth with SiO 2 colloidal coating and healed specimen, had beyond 99 % of theoretical density. Bending strength of smooth healed specimens had high strength more than 1 GPa. Crack healed specimens recovered as strength as smooth specimen, That is, cracked specimen with SiO 2 colloidal coating on cracked part recovered strength by heat treatment' completely. Crack healing of Si3N4 composite ceramics had contributed SiO 2 glassy phase and Y 2 Al 2 O- crystal phase to strength recovery.
Cited by 1 works.