저전압 지중케이블에서의 사고원인 분석

송길목, 한운기, 최명일 et al. · 한국조명전기설비학회 추계 학술발표회논문집 · 2006

The objective of this investigation was to reveal the cause of the faulted cable. For the analysis, various types or equipments such as external pattern, thermal pattern, surface structure, thermal analysis, and property distribution were deployed. The international standards and the specification provided by the manufacturer of faulted cable were examined to see if it met the standards. The following is the summary of the findings. (1) Discovered as a factor lowering insulation performance of the faulted cable: minimum thickness of the insulation layer specified by IEC 60502-1 and IEC 60811-1-1 was not met. (2) Infrared absorption peaks measured by FT-IR spectrometer revealed that the measurements made for the same material did not match and it is an important basis for proving heterogeneous composition of the insulation material. (3) It was found that PVC bedding was thermally fragile and therefore long term exposure at the site could cause similar fault pattern.