수퍼 이상 스테인리스강 용접부의 최적 열간 성형온도 및 용체화 열처리 온도에 관한 연구
지춘호, 최준태, 김대순 · 대한용접학회 특별강연 및 학술발표대회 개요집 · 2006
In order to establish the optimum hot forming temperature and solution heat treatment temperature for 25% chromium super duplex stainless steel weld, a commercial 25%Cr-10%Ni-4%Mo weld metal for super duplex stainless steel(UNS S32750) with different solution heat treatment conditions at 1100℃, 1050℃, 1025℃ and 1000℃ for 1.5 hours has been investigated by means of optical metallography, and estimated mechanical properties. It is found that exposure to elevated temperatures at 1050℃, 1025℃ and 1000℃ except 1100℃ brings partial decomposition of ferrite to austenite and sigma phase, which deteriorates their properties and heat treatment at 1100℃ shows acceptable mechanical properties.
Cited by 0 works.