폐디스크를 활용한 지오폴리머의 열적 거동 특성에 미치는 내화골재의 영향
정호준, 손세구, 김미경 et al. · 유기성자원학회 학술발표대회논문집 · 2011
In this study, we focus that high value-added recycling method for waste disc powder. For this purpose, we use metakaolin that is strong fireproof material, blast furnace slag and alkaline activators addition to waste disc powder. The experiment was estimated by compressive strength, water absorption rate, shrinkage and assessment the status of the outside according to room temperature, 500℃ and 1000℃ heat treated condition. The compressive strength from room temperature, 500℃, 1000℃ was shown 28.94~44.04㎫, 15.50~30.07㎫ and 8.95-23.14㎫ respectively. The water absorption rate between 500℃ and 1000℃ was shown similar. We suggest that the melting effect at high temperature is one major cause of a little crack and filling of internal vacant space. The shrinkage ratio at 1000℃ has measured about 2~3 fold more than 500℃ condition. We suggest that it has lower density at 500℃ condition because of low sintering temperature. And it has high shrinkage ratio at 1000℃ condition because of sintering shrinkage effect. These data related with decreased absorption rate data. At refractorly aggregate (1~3㎜) and bottom ash (3㎜) conditions, the crack occurred on outside. But in case of chamotte, sand, refractory aggregate (0.5㎜, 220F, 325F) and bottom ash (0.5㎜, 2㎜), the external crack did not occur. As a result, Thermal Stability was revealed with using waste disc and refractory aggregate even 1000℃ heat treated condition. Consequently, we can make refractory mortar. The compressive strength of metakaolin geopolymer was shown that room temperature > 500℃ > 1000℃ in order.
Cited by 0 works.