마찰교반용접한 이종간 알루미늄합금의 미세조직과 인장특성

이원준, 이효재, 박원조 · 대한기계학회 춘추학술대회 · 2012

Friction stir welding process was conducted on 5 ㎜ thick dissimilar aluminum alloys Al 2024-T3 and Al 7075-T6. And the microstructure, Vickers hardness and tensile properties were tested. 4 zones were observed through the micro structure: base material, heat affected zone, thermal mechanically affected zone and weld zone. Static strengths in such joints typically exceed 80% of the parent of the parent strength of the weaker alloy. In this study, the results showed that the yield strength and tensile strength have exceed 92% and 88%, and the weakest part of the welded material has exceed 88% of the weaker material Al 2024-T3, while the weld zone is 12% higher than the weaker material Al 2024-T3.