실구조체 크기로 제작한 전이보 매스콘크리트의 공학적 특성

윤섭, 황인성, 백병훈 et al. · 대한건축학회 학술발표대회 논문집 - 구조계 · 2004

This paper reported the results of engineering properties of mass concrete for transfer girder by using actual size specimen. For hydration heat properties, after 48 hours since placement, temperature of concrete reached up to 93℃ and temperature difference between surface and center was found to be 30℃, which caused the surface crack at top section. For compressive strength. at 28 days, core specimen had the highest compressive strength followed by standard curing specimen, field curing specimen and temperature history specimens. Temperature history specimens gained more than 39㎫ at 14days due to excessive hydration heat but above this age. additional strength gain was not achieved. For the effect of coring position on compressive strength. top section coring specimen had the highest compressive strength followed by middle section and bottom section. For the relationship between rebound value and compressive strength, good agreement was obtained. In the region of high strength. rebound number can be applicable to estimate compressive strength effectively.

Cited by 0 works.

Authors