어긋남을 갖는 맞댐용접 이음부의 인장실험

송현근, 정효원, Jee‐Hwan Kim et al. · 대한건축학회 학술발표대회 논문집 - 구조계 · 2009

The full penetration welded joint should not be gap, but the welding defects in the field are sometimes occurred. Because the strength reduction in the full penetration welded joint with gaps are expected, the allowable tolerance must be kept. This study, tensile tests on beam-beam welded joints with gaps are conducted to evaluate the relationship between tensile strength and the amount of gaps. The thickness(t) tensile specimens is 19㎜ and, SS400 class steel is used. The main variables are beveling shape(L-type, K type), unevenness(e: 0, 2, 4, 6 (㎜)), backing piece(1, 2), and the unevenness direction (up, down). And, the CO₂ gas shield arc semi-automatic welding is used. Also, the temperature of the welding between pass was less than 250 ℃. Also, comparison of a criterion and to the experiment results was performed. It is concluded that specimens with unevenness over 4㎜ on full penetration welded joint has lower yield strength, maximum strength and smaller deformation ability than a specimen with normal specimen. Afterward, studies of repairing of welded joints are required.

Cited by 0 works.

Authors