소형 굽힘 파괴인성 시편의 소성구속력 손실 보정에 미치는 구속조건의 영향
김만원, 김민철, 이봉상 · 대한기계학회 춘추학술대회 · 2006
Attention has been paid to the use of small sized specimens for the fracture toughness test of nuclear power plant materials in particular. It has been reported that the stress fields ahead of the crack tip experience a reduction of triaxiality resulting in a constraint size effect when the relevant structural dimensions are not large relative to the zone of extensive plasticity. ASTM E1921, commonly referred to as the Master Curve method, describes a test procedure for measuring the fracture toughness in the transition region for ferritic steels and impose a fracture toughness limit to address the constraint effect. The limit is related to an assumption that the specimen ligament must be large enough to ensure a condition of high crack front constraint at fracture. This requirement is concerned with a constraint limit, 30, in an expression to define a maximum measurable facture toughness, K Jc . In this study, we utilized a small-scale yielding correction method based on the micro-mechanical scaling model to adjust the constraint loss at the crack front of the small sized pre-cracked Charpy V-notch(PCVN) specimens by using the finite element analysis and post-processing of the numerical and experimental results. We also studied the effect of the constraint limit on the results of constraint loss adjustment at the small sized PCVN specimens. The results showed loss of constraint at M≤100, which is much higer than the corresponding censoring limit of M=30 in the ASTM E1291.
Cited by 0 works.