아스팔트 피막두께 변화에 따른 중온 아스팔트의 접착성질에 관한 연구
유인상, 조동우, 황성도 et al. · 한국도로학회 학술발표회 논문집 · 2011
Warm-Mix Asphalt(WMA) technologies have been developed since 15 years ago, which are internationally and domestically concerned with energy-saving and environmental-friendly technologies in public and private sectors of highway engineering. The performance of asphalt mass is traditionally evaluated by the penetration, viscosity, or Superpave tests. This research, however, is focused more on the properties depending on asphalt film thicknesses instead of evaluating asphalt mass behaviors by those tests. For this approach, a new testing protocol and analysis method are described by the bonding properties on each film thickness. This testing method and analysis tool are borrowed from those of DSR Moisture Damage test and applied by using ARES. The analysis results indicate that there is a limit film thickness between 200㎛ and 400㎛ , which causes significant changes of the properties. In addition, the results show that the property changes of Hot-Mix Asphalt(HMA) and WMA on the limit film thickness are also different. Therefore, it is suggested that the properties on thin film thicknesses between 200㎛ and 400㎛ should be considered in order to evaluate WMA properly.
Cited by 0 works.