미소접합시험과 유한요소법을 통한 섬유/에폭시 복합재의 계면 전단강도 해석
강수근, 김덕재, 최낙삼 et al. · 2006
In this study, we performed the microbond test by utilizing the microbond specimen with an epoxy micro-droplet adhered onto a carbon fiber. The interfacial shear stress distributions along the fiber/matrix interface were calculated by finite element analysis with three kinds of finite element models such as droplet model, circular model and pull-out model. Conclusions were obtained as follows. (1) Interfacial shear stress distribution showed that larger stresses were concentrated in the fiber/matrix interface for microbond test than for pull-out test. Thus, debonding at the fiber/matrix interface during microbond test was liable to occur at low load level. (2) Microbond test showed higher interfacial strength which was caused by various effects of micro-droplet geometry and size as well as stress concentration in the region contacting with the micro-vise tip.
Cited by 0 works.