지오폴리머 기술을 이용한 폐디스크의 내화몰탈 제조 및 열적 거동 특성
정호준, 손세구, 박은용 et al. · 한국폐기물자원순환학회 추계학술발표논문집 · 2011
This study is on the recycling of waste, waste of high value solutions for need improvement of recycling Coal fly ash, waste disc powder, slag and alkaline activators. And the thermal stable aggregate and reinforcement of high temperature refractory mortar are used for the purpose of the study material. The experiment was estimated by compressive strength, water absorption rate, shrinkage and assessment the status of the outside according to room temperature, 500℃ and 1000℃ heat treated condition. The compressive strength from room temperature, 500℃, 1000℃ was shown 26.22~34.12㎫, 7.33~17.557㎫ and 5.92~15.96㎫ respectively. It is highest compressive strength value that using chamotte KD-1 at 1000℃ heat treated condition. The water absorption rate from 500℃, 1000℃ was shown that 16.6~21.0%, 22.9~31.6% respectively. Because it has internal and external vacant pore and crack formation through surface water, water in hydration and out of carbonation. The shrinkage rate from 500℃, 1000℃ shown 1.9~3.3%, 2.1~3.7% respectively. Between 500℃ and 1000℃ shrinkage rate variation is few. The sand, refractory aggregate (1~3㎜, 0.5㎜, 220F, 325F) and bottom ash (3㎜) the crack occurred on outside. But chamotte, bottom ash (0.5㎜, 2㎜) the external crack did not occur. It’s possible geopolymer materialization with waste disc from physical properties in our research. We can add waste disc to mortar up to 40%. Also, geopolymer mortar with waste disc did not destroy even 1000℃ heat treated condition. Their compressive strength was revealed above 5.0㎫ in all of conditions. And we confirmed refractory mortar characteristics were revealed above 10.0㎫ compressive strength in the mortar using chamotte, refractory aggregate 220F and 325F.
Cited by 0 works.