연성 의치이장재의 온성방식이 경화반응 속도와 쇼어 경도에 미치는 영향
안현정, 한옥성, 김지우 et al. · 대한치과재료학회지 · 2010
The purpose of this study was to evaluate the setting rate and time-dependent Shore A hardness changes of the silicone-based resilient denture lining materials (Self-curing: Mucosoft ® , Sofreliner ® Tough M; Heat-curing: Mucopren ® soft, Molloplast ® B). The setting behaviors of the resilient denture liners (RDL) were evaluated using an oscillating rheometer. For Shore A hardness test, disc-shaped RDL specimens (D 35 × T 6 ㎜) were fabricated in aluminum molds. Shore A hardness was determined after 1 day and 28 days of water storage at 37±1℃ and measured using a shore A durometer. Within self-cured RDL groups, Sofreliner Tough M showed slower curing rate compared to that of Mucosoft as shown with their scorch time as 3 and 2 minutes, respectively. Their setting time was about 5 min, which is similar to that of the manufacturers’ recommended curing time. They showed similar flexibility with a resistance torque value as about 12 lb?in. Heat-cured RDLs (Mucopren ® soft and Molloplast ® B) showed significantly higher torque values (16.5 and 19.4 lbㆍin, respectively) comparing to those of self-cured RDLs (p<0.05). All the RDLs tested in this study could be classified as ISO Type A (soft), and the Shore A hardness values of the heat-cured material (Molloplast ® B, Mucopren ® soft) were significantly higher than those of the self-cured material (Mucosoft ® , Sofreliner ® Tough M)(p<0.05). For all the tested RDL groups, the hardness values measured after 28 days of water storage were similar with those measured after 1 day of water storage (p>0.05). There was a positive correlation between resistance torque values and 2 4h-5s Shore A hardness values [ r= 0 .80, p= 0.20; resistance torque = 0.82×(Shore A hardness value) - 14.11]
Cited by 0 works.