열간노출에 따른 니켈기 초내열합금의 특성 변화

유근봉, 이한상, 김두수 et al. · 대한기계학회 춘추학술대회 · 2010

The rotating components in the hot sections of land-based gas turbine are exposed to severe environment during several ten hours at above 1100℃ operating temperature. The failure mechanism of the hot gas components would be accompanied by material degradation in the properties of high temperature strength and creep rupture strength. Many hot gas components in gas turbine are made of Ni-based superalloy because of their high temperature performance. In this work, we survey the time and temperature dependent degradation of Ni-based superalloy. We prepared the specimen from IN738LC that are exposed at 871~982 ℃ in 1,000 ~ 10,000 hours. We carried out the mechanical test and microstructural observation.

Cited by 0 works.