글루콘산계 초지연제의 개발을 위한 기초적 연구

황인성, 윤섭, 백병훈 et al. · 대한건축학회 학술발표대회 논문집 - 구조계 · 2004

The objective of present paper is to develop the gluconic based super retarding admixture(GSRA) to improve the quality of existing super retarding admixture(SRA) by mixing gluconic acid, MC based viscosity enhancing admixture(VEA) with specific ratio. For fresh concrete properties, the use of gluconic acid with 0.4% exhibited an increase in slump and bleeding and a decrease in air content compared with those with plain concrete. To control increased bleeding and decreased air content by gluconic acid, use of VEA with 0.04% make the bleeding and air content of concrete with gluconic acid maintained the level of plain concrete. For setting time, final set was observed at 4-4.5 days with the presence of gluconic acid. Setting time of concrete with gluconic acid was not affected by the use of VEA. For compressive strength, compressive strength of concrete with gluconic acid increased by about 15-20% at 28days after final set compared with plain concrete. And also. compressive strength of concrete with gluconic acid was not affected by the use of VEA. In the scope of the paper, proper combination of newly developed GSRA was fixed at 1:0.l(gluconic acid:MC based VEA) to both enhance the quality of existing SRA and fluidity increase.

Cited by 0 works.

Authors