위성추력기에서 촉매유실에 따른 암모니아 해리도 변화에 대한 연구
황창환, 이성남, 백승욱 et al. · 한국추진공학회 학술대회논문집 · 2011
During the development of the iridium catalyst for domestic production, the catalyst failure, loss, sintering phenomena are observed by high pressure and temperature. By these abnormal failure of catalyst bed, the performance of thruster is degraded. To figure out the detail phenomena on the damaged catalyst bed, a numerical analysis code is developed by assuming the catalyst bed as an one dimensional porous media. The numerical analysis code is validated with experiment data. Thereby, resulting physical phenomena are examined by considering the variation of catalyst bed characteristics incurred by catalyst granule failure. Through these numerical analyses we figure out the effect of the catalyst loss on the decomposition of hydrazine and ammonia.
Cited by 3 works.