미립잠열슬러리의 물성에 관한 실험적 연구

이효진, 홍재창, 이재구 · 설비공학논문집 · 2000

The thermal conductivity and density of slurries entrained with the particles of Micro-PCM are measured with respect to its temperatures as well as concentrations. For the thermal conductivity of slurries, a device made from P.A. Hilton (Model No. H470) is adopted. There is a well-scaled 0.3㎜ gap between shells into which the slurry is injected. The temperatures of the slurry are changed to 5~25℃, for which it is controled by the supplied voltage and cooling water circulated around the outer shell. The concentrations of Micro-PCM slurries are varied from 5 wt% to 50 wt%. Some general equations such as Maxwell's equation, are evaluated for their applicability with Micro-PCM slurry. As a result, it happens to be some 20% discrepancy between the experiment and the applied equations. The density measurements of Micro-PCM slurry to its temperature and concentration are performed by hydrometer. For the experiment, tetradecane encapsulated slurry (t_m≒6℃) and a mixed wax (t_m≒50℃) are tested. The temperature changes of tetradecane are applied for 0℃ to 20℃ and a mixed wax for 20℃ to 60℃, and its concentrations are changed from 5 wt% to 30 wt%. The results are compared with a general equation and the referenced data. For the conclusion, the experimental result and a general equation are well agreed.

Cited by 0 works.

Authors