측벽형 스프링클러 헤트 디플렉터의 연속성형공정 및 응력부식특성에 관한 연구

손재원, 민인홍, 박종연 et al. · 대한기계학회 춘추학술대회 · 2002

The objective of this study is to propose a method to prevent the possible stress corrosion cracking of a horizontal side-wall sprinkler head deflector in the same atmosphere of ammonia gas as is regulated in the item No. 38 of UL (Underwriters Laboratory) 199. The finite element analysis for the progressive forming process of a sprinkler head deflector is performed to calculate the distribution of the strain and residual stress after forming process and to predict the position at which corrosion cracking may occurs under a corrosive environment. And a corrosion test is carried out for three types of specimen according to post-forming treatment, one of which is annealing, another sand blasting and the other no treatment. The observation of the test specimens with a metal microscope says that the tensile residual stress is a major factor causing corrosion cracking, and that a proper heat treatment can remove or reduce the residual stress and prevent a crack from occurring even in a severe corrosive atmosphere.

Cited by 0 works.

Authors