고온 가열시 골재 종류 변화에 따른 고강도 콘크리트의 강도 특성
김상식, 장기현, 이보형 et al. · 대한건축학회 학술발표대회 논문집 - 구조계 · 2007
Results of this experiment tests showed that all specimens, as for the properties of fresh concrete, had favorable fluidity, satisfying 600±100㎜ of slump flow. Air content was varied with aggregate types which indicated 3.0±0.5% in the specimens using granite and lime stone as a coarse aggregate, but basalt used specimens increased the value more than 80%, compared with others. This is due to the multi porous properties of the basalt. The compressive strength of all specimens was indicated at around 80㎫ at 28 elapse days, but this strength values of the specimens gradually decreased at fire circumstance. It is demonstrated that the residual compressive strength of high strength structure, which was once exposed to the fire and cooled down, is deteriorated. This is highly affected by higher temperature, so that the careful attention should be considered whether the structures could be recycled again.