Фазовые превращения при термоциклической обработке металла поверхности катания колеса
Д. А. Жуков, А. А. Соболев · CyberLeninK (CyberLeninka) · 2014
The profile of tread surface, that is regulated by the standards for geometric form and mechanical and physical properties, influences significantly on the reliability and the service time of the wheel. Existing repair modes for tread surface wheel rebuild only the geometric parameters, according to the drawing measurements. However the technology of wheel repair should provide its operational integrity during longer time period. For this purpose it was developed the method of wheel rim metal heat treatment based on forming fine-grain structure combining with compression residual stresses in metal surface layer. The purpose is achieved by cycle heat treatment with accelerated cooling before the beginning of intermediate transformation. The performed test show that, as the result of triple induction heat treatment there is a perlit grain refining for more than 10 times, residual stresses up to 500 MPa are formed in the metal surface layer, and wear resistance of hardened layer increased event at 4-7 mm of the surface layer for more than 15 %.
Cited by 0 works.