소구경 분기배관 용접부의 피로강도에 미치는 용좁부 형상 및 용접공정의 영향

백종현, 김철만, 김우식 · 대한기계학회 춘추학술대회 · 2003

S-N fatigue tests were conducted to investigate the fatigue strength of small diameter socket and butt welded joints made of carbon steels. Experimental parameters were diameter, throat depth, shape of socket welds and welding procedure. Filler used in SMAW and GTAW precedure were E9016-G with diameter of 4.0 mm and ER705-G with diameter of 2.4 mm. API 5L Gr.B pipes were adopted as a small diameter diamrter brach pipes. All socket fittings were machined from ASTM A105 carbon steel. Tensile strength was not affechted by the welding procedure. Fatigth strenhth in socket weld joints increased with increasing pipe dipe diameter, area of weld wetal and weld leg length of pipe side.

Cited by 0 works.

Authors