냉각수 중에서 가스 흡수식 냉온수기 세관의 부식거동에 관한 연구
임우조, 정기철, 윤병두 · 대한기계학회 춘추학술대회 · 2002
This paper was studied on corrosion behavior of tube for gas absorption refrigerating and hot water systems in cooling water. In the tap water at 30 ℃, polarization test of Cu, 10 % cupronickel(90-10 Cu-Ni), 30 % cupronickel(70-30 Cu-Ni) and Al-brass tube was carried out. And polarization behavior, E-I(open circuit potential-corrosion current density), anodic polarization and cyclic polarization of heat exchanger tube for absorption refrigerating and hot water systems were considered. The main results are as following: 1) Open circuit potential of 10% and 30 % cupronickel becomes Jess noble than that of Cu, and noble than that of Al-brass 2) The corrosion current density of Al-brass is high than that of 10% cupronickel and Cu in low anodic potential region, but current density of Al-brass is controlled than 10% cupronickel and Cu over 350 mV/SCE 3) The controlled effect of pitting and crevice corrosion of Al-brass is excellent than cupronickel in tap water.