재생골재를 사용한 콘크리트 배합시 적정 잔골재율에 관한 연구

최희복, 안성훈, 박희곤 et al. · 대한건축학회 논문집 - 구조계 · 2005

The fine total aggregate ratio(S/A) is important factor to acquire required slump and compressive strength in concrete. Decision of the S/A can decide easily by past experience in normal concrete, but the decision of S/A, in recycled aggregate concrete, is some difficult by insufficiency of experience and data. This research, according to S/A(42%, 47%, 52%), replacing ratio of recycled aggregate(coarse aggregate; 0%, 30%, 50%, 100%, fine aggregate; 0%, 10%, 30%, 50%, 70%, 100%) as main variables of mix design, did fluidity test in fresh concrete and compressive strength and tensile strength test at hardened concrete. Result of this research is 1) the that the proportion of fine aggregate have an effect on fluidity and compressive strength of recycled aggregate concrete is depended on the replacing ratio of aggregate, 2) it is profitable in quality of recycled concrete that the proportion of fine aggregate do by below 42% in recycled aggregate concrete.

Cited by 0 works.

Authors