[論文] 꽃건조에 적합한 실리카겔의 입도에 관한 연구
손관화 · 1994
This experiment was earned out to know what grade of silica gel is the best in drying flowers. Silica gel had the least water content and was dried fastest in 90°C among 50°C, 60°C, 70°C, 80°C, and 90°C, but It started to burn 3-4days after sililca gel weight didn't reduce any more in 80°C and 90°C. The best grade of slilca gel to dry roses(Rosa hybrida L, 'Lotte Rose') and orchids(Dendrobium 'Sabine') was 20-40 mesh grade among five grades: above 40 mesh, 20-40mesh, 16-20 mesh, 12-16 mesh, and 8-12 mesh. Among20-40 mesh silica gel, Norway silica gel(30 mesh above), and U.S.A. silica gel(20 mesh above), 20 -40 mesh was the easiest to remove the silica gel granules on the surface of both Lotte Rose and denphalae 'Ecapol' after drying.
Cited by 0 works.