Влияние температуры финишной обработки на свойства микросферического алюмохромового катализатора дегидрирования низших парафинов
О. Н. Нестеров, Svetlana R. Egorova, Giyjaz E. Bekmukhamedov et al. · CyberLeninK (CyberLeninka) · 2011
The effect of alumina support with deposited precursors of the active ingredient activation temperature in the range 700-1100 ° C on chromia-alumina catalyst performance were investigated. It was established that thermal treatment at 700-800 ° C for 4 h provides an active and stable in operation conditions light paraffin dehydrogenation catalyst
Cited by 0 works.