회분식 미분반응기를 이용한 폴리에틸렌의 열분해특성 연구

차왕석, 김상훈 · 한국신재생에너지학회 학술대회논문집 · 2005

Pyrolysis of polyethylene was carried out in the stainless steel reactor of internal volume of 40cm³. Pyrolysis reactions were performed at temperature 390-450?C and the pyrolysis product were collected separately as reaction products and gas products. The molecular weight distributions(MWDs) of each liquid product were determined by GC-SIMDIS. Molecular weight of each product were decreased wi th increase of react ion temperature and time.

Cited by 0 works.