결정질 실리콘 태양전지의 도핑 최적화를 위한 선 증착 온도에 대한 연구
최성진, 송희은, 유권종 et al. · 한국태양에너지학회 추계학술발표회 논문집 · 2010
In this paper, the optimized doping condition of mono crystalline silicon solar cells with 156 × 156 ㎟ area was studied. To optimize the pre-deposition temperature in the doping process, the other conditions except variable pre-deposition temperature were fixed. These conditions were obtained in previous studies. After etching 7 μm of the surface to form the pyramidal structure, pre-deposition temperature was changed in range of 780 ℃ to 820 ℃ with 10 ℃ increment and drive-in temperature were fixed at 865 ℃. The silicon nitride deposited by the PECVD had 75 nm thickness with 2-2.1 refractive index. The silver and aluminium electrodes for front and back sheet, respectively, were formed by screen-printing method, followed by firing in 400-425-450-550-880 ℃ five-zone temperature conditions to make the ohmic contact. Mono crystalline silicon solar cell made in 790 ℃ as the pre-deposition temperature revealed 16.9 % conversion efficiency which was best in this study. This solar cells showed 34.78 ㎃/㎠ of the current density, 629 ㎷ of the open circuit voltage and 77.1 % of the fill factor.
Cited by 0 works.