음향방출법에 의한 저항 점용접부의 파괴특성에 대한 연구
조대희, 이장규, 박성완 et al. · 한국공작기계학회 논문집 · 2007
In this paper, the acoustic emission(AE) behaviors were investigated with single- and 2-spot resistance spot welded SPCC specimens. Test specimens were welded horizontally and/or vertically according to the rolling direction of base metal in 2-spot welding. In the case of 2-spot welding, when tensile-shear test has below amplitudes: crack initiation 50~60㏈; tear fracture 40~50㏈. And when cross tensile test has below amplitudes: early stage 75~85㏈; yielding point 65~75㏈; post yielding 40~60㏈; plug fracture 70~80㏈ or 90~100㏈. Also, from the b-value that is slope of AE amplitude, we knew that there are lots of low amplitudes if b-value is big(i.e., tensile-shear specimen→tear fracture or shear fracture), and there are lots of high amplitudes if b-value is small(i.e., cross tensile specimen→plug fracture). As the results of fracture mechanism analyses through AE amplitude distributions, change of the b-value represented fracture patterns of materials. Correspondingly, low amplitude signals appeared in crack initiation, and high amplitude signals appeared in base metal fracture. We confirmed that these amplitude distributions represented the change or degradation of materials.
Cited by 0 works.