水泥固化体中Cs(上标 +)浸出行为研究
李玉香, 全明, 易发成 et al. · 2011
The leaching behavior of Cs(superscript +) in alkali-activated slag-clay minerals composite cement (AASCM) and ordinary portland cement (OPC) waste forms at temperatures of 25, 40, 70, and 90℃ was researched. The leaching mechanism was also discussed. The results indicate that the leaching behaviors of Cs(superscript +) in the AASCM and OPC waste forms are quite different. The cumulative leaching fractions (CLF) of Cs(superscript +) in the OPC waste form tend to be a same value at the four temperatures while the CLF of Cs(superscript +) in the AASCM waste form increase with increasing temperature. In the AASCM waste form, the state of adsorption/solid solution-Cs(superscript +) is about 90% and the dissolution-Cs(superscript +) is about 10%. The existent state of Cs(superscript +) in the OPC waste form mainly includes the solid solution-Cs(superscript +) and dissolution-Cs(superscript +), which are 40% and 60%, respectively.