온도에 의한 점토강화나노복합재의 인장특성 변화
하성록, 이경엽 · 한국생산제조시스템학회 학술발표대회 논문집 · 2008
Clay/epoxy nanocomposites were prepared using clay containing 6 wt%.. Tensile tests were performed using pure epoxy, and clay/epoxy nanocomposites at -30℃, 25℃(room temperature), 40℃, and 70℃ (above the glass transition temperature). Tensile strength and elastic modulus at -30℃ were higher than those at room temperature for all cases. However, tensile properties were decreased with the increase of temperature. In particular, at 70℃, tensile properties were lower than 10% of their original values at room temperature, independent of adding of the clay. The reason why tensile properties of clay/epoxy nanocomposites were increased at -30℃ was attributed to the reinforcing effect by adding of clay in the epoxy. However, at 70℃, which is above glass transition temperature of epoxy used in this study, epoxy was softened and had characteristics of rubber. The weakening effect of epoxy was greater than the reinforcing effect by clay.
Cited by 0 works.