세그먼티드 폴리우레탄 탄성체에 관한 연구 ; 디이소시아네이트로 연장된 소프트 프리폴리머 분자량에 따른 영향

도현성, 노시태 · Applied Chemistry · 2000

Segmented polyurethane elastomer(SPU) represents special material properties because of having the phase-seperated structure as a result of the thermodynamic incompatibility between soft segment (SS) and hard segment (HS). In the synthesis of SPU, we used poly (tetramethylene) glycol(PTMG, M ̄_w =2,000) as a polyol and 4,4`-diphenylmethane diisocyanate(MDI). We used 1,4-butandiol(BD) as a chain extender and N,N`-dimethylformamide (DMF) as a solvent to control the viscosity of reaction. To change the microstructure within SPU, we synthesized SPU having the respectively different contents of HS, and different ratio of [NCO]/[OH] in the step of prepolymer synthesis. In the analysis of thermal characterization of SPU using Differential Scattering Calorimeter (DSC), with increasing the ratio of [NCO]/[OH] in the prepolymer and the contents of HS in SPU, higher heat capacity in the melting temperature region could be seen.