STD11강의 상변화 및 기계적 성질에 미치는 초심냉처리의 영향

김형준, 장우양 · 열처리공학회지 = Journal of the Korean society for heat treatment · 2015

Effects of austenitizing, cryogenic treatment and tempering conditions on the phase change, microstructure and Vickers hardness value have been studied in STD11 steel for tool and die. The volume fraction of retained austenite increased with a rise in austenitizing temperature, while the volume fraction of eutectoid M7C3 carbides decreased. The retained austenite could be reduced by cryogenic treatment i.e., maintaining at LN2 temperature (-196℃) for 12hrs but a little amount of retained austenite did not transform to martensite further although holding time increased to 24 hrs or more. The microstructure of the quenched and then cryogenictreated specimen showed nano-sized and needle-shaped carbides in matrix due to the decomposition of martensite by tempering, but that of the one without cryogenic treatment still revealed retained austenite by tempering even at 500℃. (ReceWed April 29, 2015; Revised May 8,2015; Accepted May 19, 2015)

Cited by 0 works.

Authors