Теоретическое обоснование снижения износа деталей сопряжения «Поршневая канавка - поршневое кольцо»
Марьин Дмитрий Михайлович, Хохлов Алексей Леонидович, Глущенко Андрей Анатольевич · Вестник Ульяновской государственной сельскохозяйственной академии · 2015
In accordance with the second rule of the classical theory of friction based on a minimum implementation of the contactee’s body in mating surface, to reduce wear of the pair “piston groove piston ring” is proposed to increase the microhardness of the friction surface of the piston grooves of the piston internal combustion engine formation on its surface oxidized layer by the method of microarc oxidation. To establish the dependence of the microhardness of wear of the oxidized layer performed the calculation of the values of microhardness of oxidized layer piston grooves НV1 = 1100...1700 MPa with interval of 100 MPa, the microhardness of the piston ring НV2 = 1100 MPa, the details of the pair – 400 hours After the calculations revealed that in order to reduce wear of the pistons the micro hardness of oxidized surface layer friction piston grooves should be between 1250...1350 MPa. In this case, the wear of the piston grooves of the piston oxidized during the calculation period detail work mate 400 x 5.7 μm, which is 1.6 times lower than that of the piston grooves of the piston model (9.5 microns). The wear of the piston ring in oxidised piston 25.8 μm, which is 1.1 times higher than that of the piston model piston ring (23,6 μm). General wear and tear mate “piston groove piston ring is a” reduced and is 31.5 μm, while a typical pairing, the wear amounts of 33.1 μm.
Cited by 0 works.