Оптимизация процесса делигнификации древесины осины пероксидом водорода в присутствии сернокислотного катализатора

Судакова Ирина Геннадьевна, Судакова Ирина Геннадьевна, Natalia V. Garyntseva et al. · SibFU Digital Repository (Siberian Federal University) · 2013

Influence of parameters of aspen wood oxidative delignification at atmospheric pressure (temperature, composition of reaction mixture, liquid/solid ratio, time) on yield and composition of a cellulose product was defined. Оptimum conditions of delignification process which favour the high yield (58,2 % mass.) of cellulose product with low content of residual lignin (0,6 % mass.) were established: temperature 100 °С, time 4 h, concentration of hydrogen peroxide – 4 % mass., concentration of acetic acid – 25 % mass., liquid/solid ratio 10.

Cited by 0 works. Open-access PDF