연구논문 : 안경렌즈 절삭용 재료의 기계적 특성 (2)
김진구, 이영일 · 2000
β-SiC powder and α-SiC powders of different particle sizes, containing 5.7 wt% A1₂O₃ and 4.3 wt% Y₂O₃ as sintering aids, were hot - pressed at 1780℃ and subsequently annealed at 1950 to initiate grain growth. All the hot - pressed and annealed materials consisted of large SiC grains and elongated SiC grains. Typical hardness and fracture toughness of materials for spectacle lens cutting were 15.6 GPa and 5.7 MPa · ml^(1/2), respectively.
Cited by 0 works.