계면활성제를 첨가한 미셀 형성 세라믹 분리막에 의한 칼슘이온 제거

박보름, 박진용 · 멤브레인 = Membrane Journal · 2008

Sodium dodecyl sulfate, which was anionic surfactant, at a concentration higher than its critical micellar concentration was added to calcium solution for forming micelles. Then aggregates were formed by adsorption or binding of calcium ions on the surface of micelles, and gathering between them, and then rejected by two kinds of ceramic membranes to remove calcium ions. As result, rejection rates of calcium were higher than 99.98%. And in our experimental range the higher TMP trended to increase the resistance of membrane fouling (Rf), total permeate volume (VT), dimensionless permeate flux (J/Jo) and permeate flux (J) because TMP was driving force. And we investigated effects of N2-back-flushing time and filtration time, that was back-flushing period, during periodic N2-back-flushing on ceramic membranes. As result, optimal BTs for NCMT-623l (0.07 μm pore size) and NCMT-7231 membrane (0.10 μm) were 10 sec and 15 sec, respectively. Also, optimal FT was 5 min for both membranes, and the frequent N2-back-flushing could decrease membrane fouling effectively. Then, the optimal conditions resulting from our experiments for synthetic calcium solution were applied to groundwater using as washing process of soymilk package. As result, rejection rates of calcium were higher than 99.98%.

Cited by 0 works.

Authors