전기방사 방법을 이용한 천연 다당류 나노섬유 제조 및 특성 연구
김세종, 이수정, 우창화 et al. · Membrane Journal · 2016
In this study, alginate/poly(ethylene oxide) (PEO), and chitosan/PEO solution are prepared by dissolving alginate and chitosan into specific solvent for electrospinning. Solutions are poured into 10 mL plastic syringes with a metal nozzle supplied a high voltage power. The solution of alginate and chitosan is controlled by polymer concentration, temperature, relative humidity, applied voltage, distance from nozzle and flow rate of solution. Morphologies of fabricated nanofiber are observed by scanning electron microscopy (SEM). Optimal conditions for electrospinning of alginate nanofiber membrane are 2 wt% of alginate, 2 wt% of PEO at 60°C, 15 cm from the nozzle, 8 μm/min flow rate and 20~24 kV. The conditions for elctrospinning of chitosan nanofiber membrane are 2 wt% of chitosan, 2 wt% PEO at 25°C , 15 cm from the nozzle, 8 μm/min flow rate and 24 kV. The fabrication conditions of complex nanofiber prepared with chitosan and alginate are 20 cm from the nozzle, 8 μm/min flow rate and 26 kV.
Cited by 0 works.