고질소 이상 스텐레스 강의 고온시효거동
김준호, 하태권 · 한국소성가공학회 학술대회 논문집 · 2013
High temperature ageing behavior of heat-resisting duplex stainless steel for retort used in Pidgeon process for Mg production was investigated in this study. 25Cr-8Ni based duplex stainless steels were cast into rectangular ingots of which the dimension was 350×350×100mm³. Nitrogen and Yttrium were added up to 0.4 weight per cent. Phase equilibrium was calculated using the thermodynamic software FactSage® and the database of FSStel. For comparison, 310S steel, widely used heat-resisting austenitic stainless steel, was also cast in this study. Addition of N and Y had no effect on the thermal expansion behavior. High temperature tensile and compression tests were conducted on the ingots at 1230℃, which is operation temperature employed for Mg production by Silicothermic reduction. The steel with N and Y showed much higher strength than 310S in both tensile and compression tests. By thermal exposition at 1230℃ for 64 hrs, hardness of duplex stainless steel containing N and Y was found to increase, while that of 310S decreased.
Cited by 0 works.